型號(hào) | AWS | 熔敷金屬化學(xué)成分(%) | 熔敷金屬機(jī)械性能 | 用 途 | ||||||||||||
C | Mn | Si | S | P | Cr | Ni | Mo | V | R m (MPa) |
Rel或Rp0.2 (MPa) |
A (%) |
A KV (J) |
PWHT | |||
E5015-G | E7015-G | - 0.062 |
≥1.00 1.15 |
≥0.80 0.47 |
- 0.009 |
- 0.015 |
- | ≥0.50 0.70 |
- | - | ≥490 560 |
≥410 430 |
≥25 29 |
-40℃ ≥54 150 |
620℃×1h | 用于沖擊韌性有更高要求的壓力容器用低合金鋼的焊接 |
E5518-B2 | E8018-B2 | 0.05-0.12 0.080 |
≤0.90 0.73 |
≤0.80 0.24 |
≤0.020 0.009 |
≤0.030 0.013 |
0.80-1.5 1.31 |
— | 0.40-0.65 0.52 |
— | ≥540 630 |
≥440 520 |
≥19 22 |
常溫≥27 170 |
690℃×1h | 用于工作溫度520℃以下的1%鉻,0.5%鉬低合金鋼焊接 |