性能項目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機械性能 | 拉伸強度(引張強度) |
|
ASTM D638/ISO 527 | 67 | kg/cm2(MPa)[Lb/in2] |
斷裂伸長率 |
|
ASTM D638/ISO 527 |
|
% | |
拉伸模量 |
|
ASTM D638/ISO 527 |
|
kg/cm2(MPa)[Lb/in2] | |
拉伸屈服伸長率(延伸率) |
|
ASTM D638/ISO 527 | 85 | % | |
拉伸斷裂伸長率(延伸率) |
|
ASTM D638/ISO 527 |
|
% | |
彎曲模量(彎曲彈性率) |
|
ASTM D790/ISO 178 | 2740 | kg/cm2(MPa)[Lb/in2] | |
彎曲強度 |
|
ASTM D790/ISO 178 | 96 | kg/cm2(MPa)[Lb/in2] | |
洛氏硬度 |
|
ASTM D785 | 94 |
|
|
IZOD 缺口沖擊強度 | 1/4" 23℃ | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | |
1/4" -30℃ | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
1/8" 23℃ | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
1/8" -30℃ | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
Charpy沖擊強度 | 23℃ (缺口) | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
23℃(無缺口) | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無缺口) | ASTM D256/ISO 179 |
|
kg·cm/cm(J/M)ft·lb/in | ||
物性性能 | 比重(密度) |
|
ASTM D792/ISO 1183 | 1.42 |
|
成型收縮率 |
|
ASTM D955 |
|
% | |
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 |
|
g/10min | |
220℃/10kg | ASTM D1238/ISO 1133 |
|
g/10min | ||
吸水率 23℃/24H |
|
ASTM D570/ISO 62 | 0.2 | % | |
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | 130 | ℃(℉) |
未退火 | ASTM D648/ISO 75 |
|
℃(℉) | ||
維卡軟化點 |
|
ASTM D1525/ISO R306 |
|
℃(℉) | |
熔點 |
|
- |
|
℃(℉) | |
燃燒性(率) |
|
UL94 | HB |
|
|
線性膨脹系數(shù) |
|
ASTM D696/ISO 11359 |
|
mm/mm.℃ | |
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 |
|
|
1MHZ | ASTM D150/IEC 60250 |
|
|
||
體積電阻率 |
|
ASTM D257/IEC 60093 |
|
Ω.cm | |
表面電阻率 |
|
ASTM D257/IEC 60093 |
|
Ω | |
耐電弧性 |
|
ASTM D495/IEC 60112 |
|
|
|
加工條件 | 干燥條件 |
|
|
|
|
加工溫度 | 射嘴 |
|
|
℃ | |
料筒前段 |
|
|
℃ | ||
料筒中段 |
|
|
℃ | ||
料筒后段 |
|
|
℃ | ||
熔體溫度 |
|
|
|
℃ | |
模具溫度 |
|
|
|
℃ | |
壓力 | 注塑壓力 |
|
|
Mpa | |
保壓壓力 |
|
|
Mpa | ||
背壓 |
|
|
Mpa | ||
螺桿轉(zhuǎn)速 |
|
|
|
rpm | |
其他 | 備注 |
|
|||
顏色 |
|
||||
特性 | 高粘度 | ||||
用途 |
|